Title: Another Look at the Relationship between Strength and Composition of Concrete

Author(s): Sandor Popovics

Publication: Materials Journal

Volume: 108

Issue: 2

Appears on pages(s): 115-119

Keywords: cement content; composite; model; modulus; water-cement ratio

Date: 3/1/2011

Abstract:
This paper contributes to the relationship between the concrete strength and its composition by offering novel, multi-variable formulas for the concrete strength-versus-composition relationship.