Title: SP-274: Fiber Reinforced Self-Consolidating Concrete: Research and Applications

Author(s): Editors: Corina-Maria Aldea and Liberato Ferrara / Sponsored by: ACI Committee 544 and ACI Committee 237

Publication: Special Publication

Volume: 274

Issue:

Appears on pages(s): 160

Keywords:

Date: 10/1/2010

Abstract:
This symposium CD-ROM contains eight papers that were presented at technical sessions sponsored by ACI Committees 544 and 237 at the 2009 ACI Fall Convention in New Orleans, LA. The topics of the papers cover aspects ranging from mixture composition and influence of fibers on the fresh state performance to the connection between fresh state behavior, fiber dispersion and orientation and mechanical properties of the fiber-reinforced composite to full-scale testing and development of prototype applications for structures and infrastructures. Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP-274