Title: CP-45(10): Technician Workbook for ACI Certification of Aggregate Testing Technician - Level 2
Author(s):
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s):
Keywords:
Date: 1/1/2010
Abstract:
Note: A newer version of this document exists. This document was replaced by CP-45(11).
This workbook contains information about the ACI Aggregate Testing Technician – Level 2 (ATT2) certification program, performance checklists, and reprints of all the resource materials referenced by the certification examinations. The ATT2 program includes the following AASHTO and ASTM standards: T 96/C 131, C 535, T 112/C 142, D 4791, T 19/C 29, T 104/C 88, T 113/C 123, T 176/D 2419, T 304/C 1252, and D 5821.