Title: SP-267: Nanotechnology of Concrete: The Next Big Thing is Small

Author(s): Editors: Konstantin Sobolev and Mahmoud Reda Taha / Sponsored by: ACI Committee 236

Publication: Special Publication

Volume: 267

Issue:

Appears on pages(s): 180

Keywords:

Date: 10/1/2009

Abstract:
This CD-ROM consist of 9 papers sponsored by ACI Committee 236, at the Fall 2009 Convention in New Orleans, LA, in November 2009. The papers included cover a broad range of subjects related to the nanotechnology and material science of concrete with focus on nanostructure characterization, synthesis, design, and modeling of cement based materials, as well as application of nano-materials in concrete technology. Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP-267