Title: SP-266: Modeling As a Solution to Concrete Problems

Author(s): Editor: Jussara Tanesi / Sponsored by: ACI Committee 118 and ACI Committee 236

Publication: Special Publication

Volume: 266

Issue:

Appears on pages(s): 150

Keywords:

Date: 10/1/2009

Abstract:
This CD-ROM consists of ten papers that were presented by ACI Committees 236 and 188, at the ACI Fall 2009 Convention in New Orleans, LA, in November 2009. The papers cover durability models, early age models, virtual testing and mechanical behavior models. Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP-266