In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Founded in 1904 and headquartered in Farmington Hills, Michigan, USA, the American Concrete Institute is a leading authority and resource worldwide for the development, dissemination, and adoption of its consensus-based standards, technical resources, educational programs, and proven expertise for individuals and organizations involved in concrete design, construction, and materials, who share a commitment to pursuing the best use of concrete.
American Concrete Institute 38800 Country Club Dr. Farmington Hills, MI 48331-3439 USA
Phone: 1.248.848.3700 Fax: 1.248.848.3701 Staff Directory
Email Support
Feedback via Email Phone: 1.248.848.3800
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: SP-262: Ninth ACI International Conference on Superplasticizers and Other Chemical Admixtures
Author(s): Editors: P. Gupta, T.C. Holland, and V.M. Malhotra
Publication: Special Publication
Volume: 262
Issue:
Appears on pages(s): 420
Keywords:
Date: 10/1/2009
Abstract:This Symposium Publication includes 30 papers selected from a conference that took place in Seville, Spain, in October 2009. Topics include Use of a Supplemental Agent to Improve Flowability of Ultra-High Performance Concrete; Performance of Superplasticizers in Blended Cement Systems; and Multifunctional Chemical Admixture to Reduce Quality Control Requirements of Self-Consolidated Concrete. Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP-262