Lightweight Microsilica (silica fume) Concrete Use in the U.S.A.

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Lightweight Microsilica (silica fume) Concrete Use in the U.S.A.

Author(s): Mark D. Luther

Publication: Special Publication

Volume: 136

Issue:

Appears on pages(s): 273-294

Keywords: durability; high-strength concretes; lightweight aggregate concretes; lightweight aggregates; parking facilities; permeability; shales; silica fume; slates; General

Date: 1/1/1993

Abstract:
Structural Lightweight Aggregate Concrete