Title: Determining if In-Place Grout Meets Specifications

Author(s): Luke M. Snell and Robert B. Rutledge

Publication: Concrete International

Volume: 13

Issue: 1

Appears on pages(s): 29-31

Keywords: compressive strength; cores; evaluation; grout; specifications; nondestructive tests; reinforced masonry; statistical analysis; General

Date: 1/1/1991

Abstract:
Procedures to determine whether or not the compressive strength of in-place grout meets specifications are not available in the literature. Investigators are thus forced to improvise by using techniques from nondestructive testing, concrete technology, and statistics. This paper presents a procedure for locating the areas to be tested, removal of samples for testing, and a method of determining if the in-place grout meets specifications.