Title: Surface Preparation for Adhesives

Author(s): Myles A. Murray

Publication: Concrete International

Volume: 11

Issue: 9

Appears on pages(s): 69-71

Keywords: abrasive blasting; adhesives; bonding; concretes; finishes; General

Date: 9/1/1989

Abstract:
Outlines the correct way to specify the various physical and chemical methods of preparing concrete surfaces for adhesives to insure that adequate bond is achieved.