Title: O'Hare Airport Departure Ramp

Author(s): Robert I. Pearson

Publication: Concrete International

Volume: 10

Issue: 5

Appears on pages(s): 63-65

Keywords: bridge decks; concretes; latex; Construction

Date: 5/1/1988

Abstract:
When the City of Chicago expanded the upper roadway at O'Hare Airport, a latex-modified concrete overlay for the deck was specified. The decision was based on the excellent performance of the 10-year old latex-modified concrete topping on the original deck.