Title: Recycling Detroit's Lodge Freeway

Author(s): Robert I. Pearson

Publication: Concrete International

Volume: 10

Issue: 8

Appears on pages(s): 17-19

Keywords: coarse aggregates; concrete pavements; crushed concrete; recycling; Construction

Date: 8/1/1988

Abstract:
Recycling of the old reinforced concrete pavement provided more than enough coarse aggregate for the new concrete placed during reconstruction of 8.7 miles (14 km) of Detroit's John C. Lodge Freeway in 1987.