Title: Floor tolerances

Author(s): Eldon Tipping

Publication: Concrete International

Volume: 10

Issue: 6

Appears on pages(s): 51-57

Keywords: concrete slabs; evaluation; floors; measurement; specifications; tolerances (mechanics); Design

Date: 6/1/1988

Abstract:
A report on a floor profile case study of a 200,000 ftý (60,960 mý) concrete structure.