Title: Technological Aspects of Steel Fiber Reinforced Concretes

Author(s): Zygmunt Jamrozy and Jan Olek

Publication: Special Publication

Volume: 105

Issue:

Appears on pages(s): 375-390

Keywords: accelerated curing; admixtures; compacting; metal fibers; fiber reinforced concretes; fly ash; metal fibers; plasticizers; workability; Materials Research

Date: 12/1/1987

Abstract:
Paper focuses on technological aspects of steel fiber reinforced concrete (SFRC) related to the workability improvement, unconventional compaction techniques, and low-pressure steam curing. Major research data are presented, along with suggestions for future applications of some of the techniques discussed.