Title: A tribute to "Proportioning Concrete Mixtures"

Author(s): D.A. Abrams

Publication: Special Publication

Volume: 249

Issue:

Appears on pages(s): 81-92

Keywords:

Date: 3/1/2008

Abstract:
A discussion preceding a demonstration of actual field proportioning of concrete by Stanton Walker. Mr. Walker has prepared a resume of the methods used which appears on p. 182 of this volume.