Stresses in Deep Beams

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Stresses in Deep Beams

Author(s): Chow, L.; Conway, H.; and Winter, G.

Publication: 318Reference

Volume: 10

Issue: 22

Appears on pages(s): pp. 686-708

Keywords:

Date: 6/1/2005

Abstract:
Transactions, ASCE, V. 118, 1953