Title: Interesting Aspects of the Empirical Wall Design Equation

Author(s): Kripanarayanan, K. M.

Publication: 318Reference

Volume: 14

Issue: 2

Appears on pages(s): pp. 204-207

Keywords:

Date: 6/1/2005

Abstract:
ACI JOURNAL, Proceedings V. 74, No. 5, May 1977