Title: Fly Ash Increases Resistance of Concrete to Sulfate Attack

Author(s): Dikeou, J. T.

Publication: 318Reference

Volume: 4

Issue: 1

Appears on pages(s): 25 pp.

Keywords:

Date: 6/1/2005

Abstract:
Research Report No. C-1224, Concrete and Structures Branch, Division of Research, U.S. Bureau of Reclamation, Jan. 1967