Design of Deep Girders

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Design of Deep Girders

Author(s): Portland Cement Association

Publication: 318Reference

Volume: 10

Issue: 23

Appears on pages(s): 10 pp.

Keywords:

Date: 6/1/2005

Abstract:
Portland Cement Association, Skokie, Ill., 1946