Title: Strength Decay of RC Columns under Shear Reversals

Author(s): Wight, J. K., and Sozen, M. A.

Publication: 318Reference

Volume: 21

Issue: 14

Appears on pages(s): pp. 1053-1065

Keywords:

Date: 6/1/2005

Abstract:
Proceedings, ASCE, V. 101, ST5, May 1975