Title: Behavior of Interior Beam to Column Connections under Earthquake Type Loading
Author(s): Durrani, A. J., and Wight, J. K.
Publication: 318Reference
Volume: 21
Issue: 29
Appears on pages(s): pp. 343-349
Keywords:
Date: 6/1/2005
Abstract:
ACI JOURNAL, Proceedings V. 82, No. 3, May-June 1985