Title: SP-243: 9th CanMET/ACI Int Conference on Recent Advances in Concrete Technology
Author(s): Editor: V.M. Malhotra
Publication: Symposium Paper
Volume: 243
Issue:
Appears on pages(s): 150
Keywords:
Date: 4/1/2007
Abstract:
This publication contains the proceedings from the Ninth CANMET/ACI International Conference on Recent Advances in Concrete Technology, held in Warsaw, Poland, in May 2007. The nine papers include optimization of mixture proportions of normal, high-performance, and self-consolidating concrete; reactive powder concrete mixtures for producing thin precast elements; and efflorescence of concrete products for interlocking block pavements.
Note: The individual papers are also available. Please click on the following link to view the papers available, or call 248.848.3800 to order.