Title: CP-19(06): Technician Workbook for ACI Certification of Concrete Strength Technician

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s):

Keywords:

Date: 1/5/2006

Abstract:

Note: CP-19(06) is no longer available. This document was replaced by CP-19(07).

This Workbook contains information about the ACI Concrete Strength Testing Technician certification program, study questions, sample checklists, and a practice exam as well as reprints of all the resource materials referenced by the certification examinations. The CSTT program covers the following ASTM Standards: C 39, C 78, C 617, C 1231