Title: SP-054: Shotcrete for Ground Support

Author(s): Sponsored by: US DOT, ACI, SME (AIME), and Canadian Geotech Society

Publication: Special Publication

Volume: 54

Issue:

Appears on pages(s): 776

Keywords:

Date: 1/1/1977

Abstract:
SP54 Proceedings of the 1976 Engineering Foundation Conference on shotcrete. A compilation of 49 papers from 11 sessions. The major topics include: materials, field control, equipment and processes, payment provisions, design, case histories, and performance.