Title: Shear Transfer in Concrete Having Reinforcement at an Angle to the Shear Plane

Author(s): A.H. Mattock

Publication: Special Publication

Volume: 42

Issue:

Appears on pages(s): 17-42

Keywords: cracking (fracturing); loads (forces); precast concrete; reinforced concrete; reinforcing steels; research; shear properties; stress transfer; structural analysis; tests

Date: 1/1/1974

Abstract:
This paper presents and experimental and analytical study of shear transfer across a plane inclined at an arbitrary angle to a parallel or orthogonal array of reinforcement.