Title:
Variations in the Modulus of Elasticity and Poisson's Ratio with Temperature
Author(s):
J.C. Marechal
Publication:
Symposium Paper
Volume:
34
Issue:
Appears on pages(s):
495-504
Keywords:
aggregate shape and texture; aggregates; compressive strength; concretes; desorption; high temperature; hydration; low temperature; modulus of elasticity; moisture content; Poisson ratio; porphyry; quartz; research; temperature
DOI:
10.14359/18083
Date:
1/1/1972
Abstract:
Experimental results are given drawn fro the study of properties of concrete from - 160 C to + 500 C; the variations in the modulus of elasticity and the Poisson ratio varying with the change of state and temperature are discussed in relation with the other thermodynamic properties of the material.