Title: Examples of the Behaviour of Shotcrete Linings Underground

Author(s): Rolf Selmer-Olsen

Publication: Special Publication

Volume: 54

Issue:

Appears on pages(s): 722-734

Keywords:

Date: 1/1/1977

Abstract:
The following examples of the use of shotcerete are taken from a number of different tunnels and permanent underground openings in Norway.