Title: The Mechanics of Fiber Reinforcement of Cement Matrices

Author(s): R.N. Swamy, P.S. Mangat, and C.V.S.K. Rao

Publication: Special Publication

Volume: 44

Issue:

Appears on pages(s): 1-28

Keywords: bonding; cemens; cracking (fracturing); deformation; fiber reinforced concretes; flexural strength; metal fibers; reinforced concrete

Date: 1/1/1974

Abstract:
The various factors which influence the fiber reinforcement of cement matrices are briefly discussed.