Title: Thermal Properties of Refractory Castables Fired in a Temperature Gradient

Author(s): D.C. Larson and H.H. Nakamura

Publication: Special Publication

Volume: 57

Issue:

Appears on pages(s): 89-104

Keywords: bonding; refractory concretes; thermal conductivity; thermal gradient; thermal properties

Date: 1/1/1978

Abstract:
An improved technique is described to measure the high temperature thermal conductivity of refractory castables fired in a temperature gradient.