Title: Proper Vibration of Portland Cement Concrete Pavements

Author(s): T.C. Paul Teng

Publication: Special Publication

Volume: 51

Issue:

Appears on pages(s): 73-92

Keywords: air entrainment; concrete construction; concrete pavements; consolidation; continously reinforced pavements; density (mass/volume); portland cements; segregation; slump tests; vibration

Date: 1/1/1975

Abstract:
A field tests was conducted during the construction of a continuously reinforced concrete pavement to study the effect of vibration on portland cement concrete pavements.