Title: Rigid Pavement Design Charts Based on A Finite Element Analysis

Author(s): Michel Sargious and Sue K. Wang

Publication: Special Publication

Volume: 51

Issue:

Appears on pages(s): 33-50

Keywords: airports; axle loads; concrete pavements; concrete slabs; deflection; finite element method; foundations; loads (forces); modulus of elasticity; Possion ratio; research; stresses; structural analysis; subgrades

Date: 1/1/1975

Abstract:
The finite element method is used to determine the stresses and deflections in rigid pavement slabs of finite size, for both central and edge loading conditions. The main variables considered are the thickness of the slab, the modulus of elasticity of the subgrade, and the values of the load and tire pressure.