Title: Recommendations on Shear and Torsion: A Comparsion of ACI and CEB Approaches

Author(s): Paul Regan

Publication: Special Publication

Volume: 59

Issue:

Appears on pages(s): 159-176

Keywords: building codes; cracking (fracturing); loads (forces); prestressed concrete; reinforced concrete; safety factor; shear properties; structural design; torsion

Date: 1/1/1979

Abstract:
A comparision of ACI and CEB approaches to shear and torsion recommendations is presented. The author discusses the application of safety factors; shear resistance of members without shear reinforcement; reinforced concrete members with shear reinforcement; the effect of shear cracking on forces in the main reinforcement; shear resistance of concrete in short shear spans; prestressed concrete; equilibrium and compatiability torsion; designing reinforcement for torsion; and designing for combined loadings