Title: Chapter 24-Precast Concrete

Author(s):

Publication: Special Publication

Volume: 10

Issue:

Appears on pages(s): 72

Keywords:

Date: 1/1/1965

Abstract:
Precast concrete reinforced concrete cast in units which are assembled and fastened together on the job. The regular provisions for reinforced concrete thus apply except for a few specific variations.