Title: Chapter 15-General Strength and Serviceability Requirements-Ultimate Strength Design

Author(s):

Publication: Special Publication

Volume: 10

Issue:

Appears on pages(s): 41-45

Keywords:

Date: 1/1/1965

Abstract:
This chapter includes an explanation of: General Requirements; Assumptions; Safety provisions; Design strength for reinforcement; Design loads; Control of deflections; Control of cracking.