Tests of High-Range Water-Reducing Admixtures

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Tests of High-Range Water-Reducing Admixtures

Author(s): Bryant Mather

Publication: Symposium Paper

Volume: 62

Issue:

Appears on pages(s): 157-166

Keywords: admixtures; air-entrained concretes; bubbles; concrete durability; concretes; freeze-thaw durability; laboratories; plasticizers; tests; water-reducing agents

Date: 1/1/1979

Abstract:
At the Waterways Experiment Station, four high-range water-reducing admixtures were tested for compliance with the requirements for water-reducing admixtures given in ASTM: C 494-71. None passed the test for frost resistance; all met all other requirements.




  