Title: Steel Fibrous-Ductile Concrete Joint for Seismic-Resistant Structures

Author(s): C.H. Henager

Publication: Special Publication

Volume: 53

Issue:

Appears on pages(s): 371-386

Keywords: bems (supports); columns (supports); cyclic loads; costs; ductility; earthquake resistant structures; earthquakes; fiber reinforced concretes; joints (junctions); loads (forces); metal fibers; reinforced concrete; reinforcing steels; stirrups

Date: 1/1/1977

Abstract:
Tests were made of ductile concrete joint designed to minimize steel congestion common to seismic-resistant building joints. An experimental comparision was conducted on two, full-sized, beam-column joints.