Title: Strength and Ductility of Cast-In-Place Beam-Column Joints

Author(s): S.M. Uzumeri

Publication: Special Publication

Volume: 53

Issue:

Appears on pages(s): 293-350

Keywords: anchorage (structural); beam-column frame; beams (supports); bond (concrete to reinforcement); columns (supports); confined concrete; connections; deflection; ductility; dynamic loads; earthquake resistant structures; earthquakes; flexural strength

Date: 1/1/1977

Abstract:
The results of an experimental study of the behavior of cast-in-place reinforced concrete beam-column joints, subjected to slow load reversals simulating seismic loading are presented.