Title: Predicting the Earthquake Response of Reinforced Concrete Structures

Author(s): Ray W. Clough

Publication: Special Publication

Volume: 53

Issue:

Appears on pages(s): 59-80

Keywords: computer programsl cyclic loads; dynamic structural analysis; dynamic tests; earthquake resistant structures; earthquakes; loads (forces); mathematical models; reinforced conrete; stiffness structural analysis

Date: 1/1/1977

Abstract:
Formulation of the dynamoc response equations for structures subjected to earthquakes is summarized, and techniques of accounting for the nonlinear cyclic loading behavior of reinforced concrete are mentioned.