Title: Design of Concrete Mixtures

Author(s): Duff A. Abrams

Publication: Symposium Paper

Volume: 52

Issue:

Appears on pages(s): 309-330

Keywords:

Date: 1/1/1976

Abstract:
The design of concrete mixtures is a subject of vital interest to all engineers and constructors who have to do with concrete work. . .The term "Design" is used in the title of this article as distinguished from "proportioning" since it is the intention to imply that each element of the problem is approached with a delibrate purpose in view which is guided by a rational method of accomplishment.




  