Title: Freeze-Thaw and Acid Resistance of Polymer-Impregnated Concrete

Author(s): Glenn William DePuy

Publication: Symposium Paper

Volume: 47

Issue:

Appears on pages(s): 233-258

Keywords: acid resistance; air entrainment; chemical attack; compressive strength; deterioration; durability; freeze-thaw durability; impregnating; modulus of elasticity; polymer-cement concrete; protective coatings; sealers; tensile strength

DOI: 10.14359/17613

Date: 1/1/1975

Abstract:
The developmental program for concrete-polymer materials has shown polymer-impregnated concrete to have significantly improved durability and strucutural properties aas compared with conventional concrete.




  