Title: Useful Techniques in Direct Modeling of Reinforced Cocnrete Structures

Author(s): Weldon W. Aldridge and John E. Breen

Publication: Symposium Paper

Volume: 24

Issue:

Appears on pages(s): 125-140

Keywords: aggregate gradation; beams supports; bond (concrete to reinforcement); compressive strength; concretes; cylinders; flexural tests; folded plates; loads (forces); micro-concrete; models; reinforced concrete; reinforcing materials; reinforcing steels

Date: 1/1/1970

Abstract:
Several useful techniques in direct modeling of reinforced concrete structural systems are described.




  