Title: Computation of Deflections for Beams and One-Way Slabs

Author(s): C.G. Salmon, A. Fattah Shaikh, and M. Saeed Mirza

Publication: Symposium Paper

Volume: 43

Issue:

Appears on pages(s): 15-54

Keywords: beams (supports); compressive strength; concrete slabs; continuous beams; cracking (fracturing); creep properties; deflection; flexural strength; loads (forces); modulus of elasticity; moments of interia; reinforced concrete; reviews; shrinkage

Date: 1/1/1974

Abstract:
The paper presents a condensed state-of-the art report on practical procedures for computing short-time and long-time deflections for beams and one-way slabs.




  