Shearing Strength and Cracking in Two-Way Slabs Subjected to Concentrated Load

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Shearing Strength and Cracking in Two-Way Slabs Subjected to Concentrated Load

Author(s): Yoshinori Aoki and Hiroshi Seki

Publication: Special Publication

Volume: 30

Issue:

Appears on pages(s): 103-126

Keywords: concrete slabs; cracking (fracturing); crack width and spacing; deflection; diagonal tension; failure mechanisms; flexural strength; reinforced concrete; research; shear strength; strength; structural design; two-way slabs; yield-line method

Date: 1/1/1971

Abstract:
This paper describes the experimental and theoretical study on ultimate strength of reinforced concrete slabs supported on beams as the boundary condition.