Corrugated Rubber Gland Strips for Sealing Bridges

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Corrugated Rubber Gland Strips for Sealing Bridges

Author(s): A. Craig Roland

Publication: Special Publication

Volume: 70

Issue:

Appears on pages(s): 1023-1038

Keywords: bridges (structures); evaluation; joint sealers; joints (junctions); performance; quality control; rubber; sealing

Date: 1/1/1981

Abstract:
The resources devoted to the develop,emt of continuous sealing glands in the last two decades have in themselves given a vote of confidence to the merits of solving joint sealing problems in bridges with this approach.