Title: Durability and Performance Criteria of Building Sealants

Author(s): Julian R. Panek

Publication: Special Publication

Volume: 70

Issue:

Appears on pages(s): 917-938

Keywords: criteria; durability; joint sealers; joints (junctions); performance; plastics, polymers and resins; specifications; structural design; tests; waterproofing

Date: 1/1/1981

Abstract:
Properly formulated sealants - applied by reputable applicators - following recommendations by the sealant manufacturer - should perform at least 20 years - when the sealants are used within their movement capability.