Title: Epoxy Polymer Modified Concretes

Author(s): R.A.V. Raff and Helen Austin

Publication: Special Publication

Volume: 40

Issue:

Appears on pages(s): 339-346

Keywords: aggregates; cement pastes; compressive strength; curing; epoxy resins; flyash; freeze-thaw durability; hydration; impregnating; mix proportioning; plastics; polymer cement concrete; portland cements

Date: 1/1/1973

Abstract:
Polymer cement concretes prepared by substituting at least 20 percent of expoxy resin for cement into ordinary Portland cement concrete mixes showed increased compressive strengths. The addition of flyash to the epoxy cement mixes increased the compressive strength further. Preliminary tests indicated that the presence of the epoxy resin does not inhibit the hydration of the Portland cement.