Polymer Impregnated Concrete As a Composite Material

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Polymer Impregnated Concrete As a Composite Material

Author(s): A. Auskern and W. Horn

Publication: Special Publication

Volume: 40

Issue:

Appears on pages(s): 223-246

Keywords: aggregates; bonding; cements; compressive strength; concretes; cracking (fracturing); density (mass/volume); failure mechanisms; hardened paste structure; impregnating; modulus of elasticity; mortars (material); polymer concrete

Date: 1/1/1973

Abstract:
The incorportation of a relatively small volume of a rigid polymer in the pore structure of concrete results in a significant increase in the elastic and mechnical properties of the material.