Development of Polymer-Impregnated Concrete As a Construction Material for Engineering Projects

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Development of Polymer-Impregnated Concrete As a Construction Material for Engineering Projects

Author(s): G.W. De Puy and J.T. Dikeou

Publication: Special Publication

Volume: 40

Issue:

Appears on pages(s): 33-56

Keywords: bridge decks; compressive strength; concrete durability; concrete pipes; concrete technology; creep properties; curing; impregnating; mix proportioning; modulus of elasticity; permeability; polymer-cement concrete; polymer concrete; precast concrete

Date: 1/1/1973

Abstract:
The developmental program for polymer-impregnated concrete (PIC) has shown that a material of greatly improved properties, as compared with conventional concrete, can be routinely produced.