Title: Concrete Structures and Construction Vibrations

Author(s): Kenneth P. Akins, Jr., and Donald E. Dixon

Publication: Special Publication

Volume: 60

Issue:

Appears on pages(s): 213-249

Keywords: autogenous healing; blast loads; concrete construction; concretes; damage; field tests; fresh concretes; pile driving; shock mechanics; structures; vibration (fresh concrete); vibrations

Date: 1/1/1979

Abstract:
Reliable methods for establishing limits on construction-related vibrations to minimize damage have been developed through the efforts of researchers.