Title: Crack Width Control in Welded Fabric Reinforced Centrally Loaded Two-Way Concrete Slabs

Author(s): Edward G. Nawy

Publication: Special Publication

Volume: 20

Issue:

Appears on pages(s): 211-236

Keywords:

Date: 1/1/1968

Abstract:
Most existing research deals with crack width studies in beams and one-way members. This investigation covers the effect of two-way action on crack width development, crack pattern evaluation and crack width control.