Title: Cracking Induced by Enivronmental Effects

Author(s): Bryant Mather

Publication: Special Publication

Volume: 20

Issue:

Appears on pages(s): 67-72

Keywords:

Date: 1/1/1968

Abstract:
When concrete cracks as a result of its interaction with its environment, and the cracking is an undesirable feature of the history of the concrete, the occurrence represents the consequences of an imperfect choice in selecting the particular concrete that was produced for service in the enviornment in which it was used.